化學(xué)配方數(shù)據(jù)庫
配方類型: COATINGS
配方說明: Gun Stock Varnish (Tung Oil 600)
配方組成: Heat to 400 and hold until 0.5 tube light with Z-3 then cool to
380 when 1.5 bubbles light, cool to 350 when 1 bubble light cool and
cest
Z-3-Z4 Bodied Tung oil/43.5
Cobalt Naphthenate (3% Co)/0.4
Mineral Spirits/54.5
"Exkin" #2/0.4
Cooking Time/4-5 hours
Lead Naphthenate (12% Pb)/1.2
配制方法: The above intermediate will make approximately 1340 lb. Use a soft rag to apply the above coating. Rub in well and allow 24 hr to dry.
Apply 3 or more coats to bring out the full lustre and grain of the wood.